  1. ASTM D698 vs D1557 | Eng-Tips

    Sep 23, 2024 · D698 is generally used for "thin" fills beneath structures. D1557 is used for airport runways, highways and "deep" fills beneath buildings. Ron is right about the …

  2. ASTM D-698 or D-1556 Proctor Method | Eng-Tips

    Does Proctor ASTM D-698 soil compaction call for 95% dry density or is that Proctor ASTM D-1156? Thank you.

  3. Compaction and ASTM D-698 Standard Proctor | Eng-Tips

    Oct 10, 2007 · Ladies and Gentlemen, I have a basic understanding of ASTM D-698 and how the test is performed and how the numbers are calculated. At my firm we usually have notes similar to "The fill …

  4. When to use ASTM D4253 & D4254 | Eng-Tips

    Jan 14, 2011 · When and why would one use ASTM D4253 or D4254 for determining density? The specification I’m looking at lists these along with the ASTM D698 and I’m unfamiliar with 4253&4254. …

  5. Is it possible to compact soil to 100% as per ASTM D698?

    Jul 24, 2018 · For what types of subgrade is it required? You see 100% of D698 or 1557 typically for sensitive pavement structures, like an airport runway, or in areas where a structure will rely on …

  6. Proctor Testing Methods | Eng-Tips

    Oct 6, 2010 · What is the basic determination of what testing method to use. Example AASHTO T-99 vs ASTM D1557. Is it size of material from the borrow site?

  7. Selection of method in AASHTO T99 | Eng-Tips

    May 18, 2005 · I know that ASTM D698/ 1557 has instructions for when to use each method, but they only have three methods, not the 4 of AASHTO. I used to think that AASHTO and ASTM were …

  8. Standard or Modified Proctor Density? | Eng-Tips

    Feb 3, 2016 · Get a copy of each standard (ASTM D698 for standard Proctor and ASTM D1557 for modified Proctor) and read it. Read corresponding in-place density test standards as well.

  9. Pipe Bedding layer: sand vs gravel | Eng-Tips

    Sep 8, 2021 · percent of ASTM D698 maximum density. Plastic piping shall have bedding to spring line of pipe. Provide ASTM D2321 materials as follows: a. Class I: Angular, 6 to 40 mm 0.25 to 1.5 …

  10. AASHTO T99 | Eng-Tips

    Aug 10, 2006 · I have aquestion that we correct max dry density vs. moisture content curve for +4 material in ASTM D698-what is in AASHTO T-99? Do we also correct the curve in AASHTO T99 or …